Material Characteristics Relevant to Aerospace Use
Titanium tube for aerospace service is chosen for four properties that act together. Titanium alloys have high specific strength, so a tube can carry a given working pressure with a thinner wall and lower mass than a steel tube of the same size. The density of titanium is about 4.51 g/cm3, roughly 57 percent that of steel, which reduces the weight of every tube run in the aircraft. Titanium is fully resistant to chloride and seawater attack, so hydraulic and fuel lines do not corrode from condensate or from de-icing salt. And the material retains useful strength at elevated temperature, which allows tube runs near engine and bleed air zones that would require insulation or a heavier material if steel were used.
Grade 2 under ASTM B338 has a UNS number of R50400 and is the most widely used unalloyed titanium grade, with a minimum tensile strength of 345 MPa and a minimum yield strength of 275 MPa in the annealed condition.
Properties Compared with Other Structural Metals
| Property | Titanium Gr2 | Ti-6Al-4V | Carbon steel | Type 304 stainless steel |
|---|---|---|---|---|
| Density, g/cm3 | 4.51 | 4.43 | 7.85 | 7.90 |
| Melting point, °C | About 1668 | About 1650 | About 1530 | About 1400 to 1450 |
| Modulus of elasticity, GPa | About 105 | About 113 | About 206 | About 200 |
| Thermal conductivity, W/(m·K) | About 17 | About 7.5 | About 63 | About 16 |
| Corrosion in chlorides | Fully resistant | Resistant, crevice sensitive | Rapid attack | Pitting and crevice attack |
The high melting point and modest thermal conductivity are the reasons titanium welds need inert gas protection for longer than steel does, and the comparatively low modulus is why a titanium tube run is more flexible and has a lower natural frequency than the steel equivalent, which has to be allowed for in support spacing.
Aerospace Applications
Hydraulic and pneumatic lines, where tubing is bent to complex routes with flareless or flared fittings and must resist both fatigue and hydraulic fluid.
Fuel and vent lines, where weight saving over the whole aircraft is significant and chloride corrosion from fuel or environment is a concern.
Bleed air and moderate temperature ducting behind engine and environmental control zones, where Grade 2 gives a usable strength margin at temperature.
Structural tube for brackets, struts and fairing supports where stiffness rather than ultimate strength governs the design.
Ground support and test rig hardware, where a clean, non-corroding and non-magnetic tube is preferred.
Fabrication and Installation Practice
Aerospace tube is normally bent on CNC tube benders with mandrels to hold ovality and wall thinning within limits, then end formed for flaring, beading or welding. Because titanium work hardens, the bend radii and the number of forming operations are planned with intermediate anneals where necessary. Cleanliness is critical: tube is cut and deburred with dedicated tooling, because iron contamination from a steel brush or a grinding wheel creates corrosion initiation sites that survive passivation. After forming, bends are stress relieved and internally cleaned to remove lubricant and debris.
Welding is by orbital or manual tungsten inert gas with full argon shielding of the weld pool and the bore. Weld colour is the field acceptance criterion: silver and light straw are acceptable, blue and grey mean contamination and are rejected. Where tube connects to aluminium or steel structure, insulating or transition fittings are used to prevent galvanic attack of the less noble metal in wet or condensation exposed areas.
Inspection and Quality Records
Seamless aeronautical tube is delivered with a chemical analysis covering interstitial elements, tensile and hardness results in the annealed condition, flattening and flare test results, hydrostatic or pneumatic pressure test records, eddy current examination of the tube body and ultrasonic inspection where specified. Positive material identification is used to verify grade at goods-in, and dimensional inspection covers outside diameter, wall thickness, ovality, straightness and length. Certification is provided to EN 10204 3.1 with full heat number traceability, and third party or customer witnessed inspection can be arranged for programme orders.
Frequently Asked Questions
Q: Why is Grade 2 used in aerospace rather than Grade 1?
A: Grade 2 has a higher minimum tensile strength of 345 MPa against 240 MPa for Grade 1, which gives a better strength to weight ratio for pressurised and structurally loaded tube while retaining excellent formability and weldability.
Q: How much weight does titanium tubing save compared with steel?
A: Titanium has a density of about 4.51 g/cm3 versus 7.85 g/cm3 for steel, so a titanium tube of identical dimensions weighs roughly 43 percent less.
Q: What pressure testing is applied to titanium tube?
A: Hydrostatic or pneumatic pressure testing of each tube or lot, with the test pressure and hold time recorded on the inspection certificate, supported by eddy current or ultrasonic examination.
Q: Why does alloy steel tube corrode where titanium does not?
A: Titanium forms a stable, self-repairing oxide film that is immune to chloride attack, whereas steel and stainless steel suffer rust, pitting and crevice corrosion in the same wet chloride environment.
Q: How is titanium tube kept clean during fabrication?
A: By using dedicated cutting and deburring tooling, avoiding steel brushes and grinding wheels, and cleaning and passivating the tube internally before assembly.