Feb 23, 2024 Leave a message

Effect Of Forging Process On The Organisation And Properties Of Titanium Rods

The materials used for forging titanium rods are mainly pure titanium and titanium alloys of various compositions, and the raw state of the materials are titanium rods, ingots, metal powders and liquid metals. The ratio of the cross-sectional area of the metal before deformation to the cross-sectional area after deformation is called the forging ratio. Correct choice of forging ratio, reasonable heating temperature and holding time, reasonable beginning and end forging temperature, reasonable amount of deformation and deformation speed to improve product quality and reduce costs have a great relationship. General small and medium-sized forgings are round or square bars as blanks. The grain structure and mechanical properties of the bar is uniform, good, accurate shape and size, good surface quality, easy to organise mass production. As long as the heating temperature and deformation conditions are reasonably controlled, no need for large forging deformation can be forged with excellent performance forgings. In the aircraft, titanium alloy is mainly used to manufacture beams, landing gear, paddle hubs and joints and other major force components; in the engine titanium alloy is mainly used to manufacture the adapter ring, the bane of the wheel fan, the pressurised discs and blades and other force and heat parts.

Titanium alloy is very sensitive to forging process parameters, forging temperature, deformation, deformation and cooling rate changes will cause changes in the organisational properties of titanium alloy. In order to better control the organisational properties of forgings, in recent years, advanced forging technologies such as hot die forging and isothermal forging have been widely used in the forging production of titanium alloys. Using conventional forging process methods, generally speaking, titanium alloys can make after forging components to obtain isometric organisation, so as to have high room temperature type and strength. For the solution of large and complex titanium bar precision forgings forming provides a viable method. This method has been widely used in titanium bar production. One of the effective ways to improve the fluidity of titanium rods and reduce the deformation resistance is to increase the preheating temperature of the mould. Isothermal die forging and hot die forging developed in the last 20 to 30 years at home and abroad.

How to improve the yield of the production of titanium rods, which can be when the use of closed die forging method of die forging titanium rods, closed die forging must be strictly limited to the volume of the original blank, which complicates the preparation process. Whether to use closed die forging, from the profit and process feasibility of both considerations. Subsequently only heat treatment and cutting blanks. The forging temperature and the degree of deformation are the basic factors determining the organisation and properties of the alloy. Heat treatment of titanium rods is different from that of steel, and die forging is usually used to produce near-scrap in shape and size. The organisation of the alloy does not play a decisive role. Therefore, the process specification of the final step of the titanium bar has a particularly important role. Must make the overall deformation of the blank is not less than 30% of the deformation temperature does not exceed the phase transition temperature, in order to make the titanium bar at the same time to obtain high strength and plasticity and should strive to temperature and deformation in the whole deformation of the blank as far as possible in the distribution of uniform.

After recrystallisation heat treatment, titanium rods and performance uniformity than steel forgings. Metal intense flow area of its low times for fuzzy crystals, high times for isometric fine crystals; difficult to deform the area, due to deformation of small or no deformation, its organisation tends to keep the state of deformation before the state. Therefore, in the die forging some important titanium bar parts (such as compressor discs, blades, etc.), in addition to controlling the deformation temperature below TB and the appropriate level of deformation, control of the original billet organisation is very important, otherwise, coarse crystalline organisation or some of the defects will be inherited into the forging, and its subsequent thermal disposal can not be eliminated, will lead to forging scrapped.

Thermal effect of local concentration of sharp deformation in the region of the hammer when die forging complex shape of titanium bar forgings. Even if the heating temperature is strictly controlled, the temperature of the metal may still exceed the alloy's TB for example, die forging cross-section for the I-beam titanium bar blanks, the hammer is too heavy, the middle (web area) local temperature due to deformation of the thermal effect of the role of the edge of the local high of about 100 ℃. In addition, difficult to deform the region and have a critical deformation level region, die forging after the heating process is easy to form plasticity and endurance strength are relatively low coarse crystal organisation. Therefore, hammer die forging complex shape forgings, its mechanical properties are often very unstable. But will lead to a sharp increase in deformation resistance, reduce the die forging heating temperature, although it can eliminate the risk of local overheating of the blank. Increase tool wear and power consumption, but also need to use more powerful equipment. Open die forging, burr loss accounted for 15-20% of the weight of the blank clamping part of the process of waste (if necessary according to the conditions of die forging to leave this part) accounted for 10% of the weight of the blank burr relative loss of metal is usually with the reduction in the weight of the blank and increase, some structural asymmetry, large differences in cross-sectional area and the existence of difficult to fill the local forging, burr consumption can be as high as 50% of the closed die forging, although there is no burr loss, but the blank making process complexity and power consumption. Closed die forging although no burr loss, but the billet making process is complex, need to add more transition grooves, will undoubtedly increase the auxiliary costs.

Send Inquiry