1, every half a month on the titanium coiler rag to wipe off the dust;
2, the product process determines its limitations performance: wall thickness is not uniform, low brightness of the inner appearance of the tube, high cost of sizing, and the inner and outer appearance of the pockmarks, black spots are not easy to remove; you can use water to clean.
3, titanium coiler testing and trimming to offline processing. Therefore it embodies its good performance in high-pressure, mechanical structure materials, do not use alcohol scrubbing.



4, the material of the product under the action of the flow force elastic and plastic strain, if the stress is large enough to lead to fracture. Clean up the product attention channel; pay attention to the interface.
5, do not let the titanium coiler catch to the acidic medium; encounter acidic medium, stainless steel will corrode.