Oct 16, 2025 Leave a message

ASTM-B337.pdf

ASTM B337 UNS R56400 Grade 5 Titanium Alloy Round Tubes

What ASTM B337 Covers

ASTM B337 is the standard specification for welded titanium and titanium alloy pipe, covering pipe made with or without filler metal and in sizes normally above those of tube. Grade 5, UNS R56400, is the alpha-beta Ti-6Al-4V alloy and is the highest strength grade routinely supplied under this specification. Because the pipe is welded rather than seamless, the specification places particular emphasis on weld quality, on the annealing condition of the finished product and on the tests that demonstrate the seam is sound.

Chemistry, Mechanical Limits and Structure

The alloy contains 5.5 to 6.75 percent aluminium and 3.5 to 4.5 percent vanadium, with maximum oxygen of 0.20 percent, nitrogen 0.05 percent, carbon 0.08 percent, hydrogen 0.015 percent and iron 0.30 percent. Minimum room temperature properties are 895 MPa (130 ksi) tensile strength, 828 MPa (120 ksi) 0.2% offset yield strength and 10 percent elongation in 50 mm. At ambient temperature the beta phase content lies between roughly 10 and 50 percent, which is what makes the alloy heat treatable, and the structure responds to solution treatment and aging as well as to simple annealing.

Property ASTM B337 Grade 5 Requirement
Tensile strength, min 895 MPa (130 ksi)
Yield strength, 0.2% offset, min 828 MPa (120 ksi)
Elongation in 50 mm, min 10%
Iron, max 0.30%
Hydrogen, max 0.015%

Applications in Marine, Offshore and Power Work

Seawater cooling and firefighting mains on ships and offshore structures.

Structural piping systems where a lighter tube reduces support steel and top weight.

Aerospace ground support and test rig pipework that must resist hydraulic fluid and salt spray.

Condenser and heat exchanger connections in power generation stations.

Chemical and desalination plant piping subject to chlorides and mildly reducing media.

The alloy is also used for bushing and hexagonal section pipe, and it has good hot forming characteristics. Cold forming is possible but demands more force and more intermediate annealing than the commercially pure grades.

Welding Grade 5 Pipe and Managing Weld Ductility

The chief fabrication risk with Ti-6Al-4V pipe is ductility loss in the weld and heat affected zone. The weld cools quickly from above the beta transus, producing a hard, less ductile structure, so procedures are written to keep heat input in a narrow band, maintain interpass temperature control and protect the weld until it drops below about 400 C. Argon shielding is specified at 99.99% purity or better, with a monitored internal purge and non permeable gas lines. Where the joint will see fatigue or thermal cycling, a post weld stress relief between 540 and 650 C restores toughness and dimensional stability. Creep strength is lower than that of the near alpha alloys, so long term service temperatures are generally kept below about 400 C, and the alloy is not selected for sustained high temperature creep duty.

Sizes, Inspection and Delivery

Standard production covers nominal bores from about 15 mm to 150 mm in schedules 10, 40, 80 and 160, with wall thickness from roughly 1 mm to 20 mm and single random, double random or cut lengths. Surface condition is cold finished, bright, polished, annealed or pickled as ordered. Inspection includes spectrographic chemical analysis, tensile testing, flattening or bend testing, hydrostatic pressure testing, ultrasonic or radiographic examination of the longitudinal seam, and hardness checks across the weld. Marking shows the standard, grade, size, wall, length and heat number, and each shipment is released with an EN 10204 3.1 mill test certificate. Additional tests such as intergranular corrosion assessment or positive material identification are available for specification driven projects.

Frequently Asked Questions

Q: Is ASTM B337 for seamless or welded pipe?

A: It is the specification for welded titanium and titanium alloy pipe. Seamless pipe in the same alloy is ordered to ASTM B861 and heat exchanger tube to ASTM B338.

Q: Why does the weld lose ductility?

A: The weld cools rapidly from the high temperature beta phase and forms a harder structure than the parent metal. Controlled heat input, correct shielding and post weld stress relief limit the effect.

Q: How strong is Grade 5 pipe compared with Grade 2 pipe?

A: Grade 5 requires 895 MPa minimum tensile strength against 345 MPa for Grade 2, so it is more than twice as strong and can be used with a substantially thinner wall.

Q: Can Grade 5 pipe be used at high temperature?

A: It is used up to about 400 C for continuous service. Its creep resistance is lower than the near alpha alloys, so higher temperature duty calls for a different grade.

Q: What tests prove the welded seam is sound?

A: Flattening or transverse bend tests demonstrate ductility of the weld, and hydrostatic pressure testing plus ultrasonic or radiographic examination confirm freedom from harmful defects along the seam.